Finland/Sweden
See below
Reports for Focus area: Granular
See below
Overview of HVS tests in Finland and Sweden 1997-2004
Test |
Start, yy/mm, duration |
Total number of loadings (10 3 ) |
Description |
Reference |
FIN01 |
97/ |
1,710 |
Base course test with low quality base |
Finnra report 30/2001 Matti Huhtala, Jari Pihlajamäki and Janne Sikiö
|
FIN02 |
97/ |
170 |
Base course test with high quality base |
|
FIN03 |
97/ |
1,400 |
Loading mode test, single wheel, bi-directional |
|
FIN04 |
97/ |
318 |
Loading mode test, single wheel, uni-directional |
|
FIN05 |
97/ |
Not started |
Loading mode test, dual wheel, bi-directional |
|
FIN06 |
98/04 1 month |
4.9 |
Thawing test, frost-susceptible subgrade |
Finnra report 31/2000 Heikki Kangas, Heikki Onninen and Seppo Saarelainen
|
FIN07 |
98/05 1 month |
8.1 |
Thawing test, frost-susceptible subgrade |
|
FIN08 |
98/05 1 month |
6.5 |
Thawing test, frost-susceptible subgrade, steel grid in base course |
|
FIN09 |
98/06 2 months |
130 |
Heavy traffic road, traditional structure |
Finnra reports 29/2001 Jari Pihlajamäki and Janne Sikiö
|
FIN10 |
98/08 2 months
|
500 |
Heavy traffic road, high resistance to fatigue structure |
|
SE01 |
98/12 |
2,296 |
The first test in a series of three with gradually increasing bearing capacity. |
Accelerated load testing of pavements VTI Report 477A
|
SE02 |
99/06 |
1,135 |
The second test in a series of three with gradually increasing bearing capacity. |
|
SE03 |
99/09 |
800 |
Maintenance treatment on SE01. |
|
SE04 |
99/12 |
165 |
Maintenance treatment on SE02. |